Send Message
Home ProductsMetal Alloy

High Performance Calcium Silicon Alloy , Metal Core Wire For Steel Melting

Certification
China Winlands limited certification
China Winlands limited certification
I'm Online Chat Now

High Performance Calcium Silicon Alloy , Metal Core Wire For Steel Melting

High Performance Calcium Silicon Alloy , Metal Core Wire For Steel Melting
High Performance Calcium Silicon Alloy , Metal Core Wire For Steel Melting

Large Image :  High Performance Calcium Silicon Alloy , Metal Core Wire For Steel Melting

Product Details:
Place of Origin: CHINA
Brand Name: HOPES
Certification: CCIC
Model Number: CaSi
Payment & Shipping Terms:
Minimum Order Quantity: 20mt
Packaging Details: steel cages on wooden (or steel) pallets, plastic shrink wrapped, labeled. Or by customer's requirment.
Delivery Time: 20 days
Supply Ability: 500-1000mt/month

High Performance Calcium Silicon Alloy , Metal Core Wire For Steel Melting

Description
Material: Metals ,Calcium , Silicon Alloy Or Not: Is Alloy
Application: Stell Melting ,Industry Shape: Cored Wire
High Light:

ferro silicon inoculant

,

high carbon silicon

High Performance Calcium Silicon Metal Cored Wire for Steel Melting

 

Cored wire in the ladle refining process has been widely used, will be pulverized into a certain size of the powder additive package (deoxidizer, desulfurization agent, alloy) wrapped in a narrow strip of continuous formation of a linear material, and its Winding into coils, according to the different core powder, cored wire features and uses are different.

Cored wire is mainly used in steelmaking, which can purify the shape of steel inclusions, play the role of pure molten steel and partly change the nature and shape of inclusions, improve the quality of molten steel, improve the casting state, improve the castability of steel and improve the use of steel Performance, and can significantly improve the yield of the alloy, reduce alloy consumption, reduce the cost of steelmaking.

As Cored wire is condutive to the adjustment and control of the content of easily oxidizable elements and trace elements, it can greatly improve the yield of the alloy, reduce the smelting cost, shorten the smelting time and precisely control the composition.

Designation Chemical Composition(%) Wire Dlameter Wire Thickness Wire Weight Powder Weight Unlformlty
mm mm g/m g/m %
SiCa Si Ca 13-13.5 0.35 145 230 2.5-5
55 30
CaAl Ca Al 13-13.5 0.35 145 210 2.5-5
26-30 3-24
Ca Ca 13-13.5 0.35 145 125 2.5-5
28-35
SiCaBa Si Ca Ba 13-13.5 0.35 145 220 2.5-5
55 15 15
SiAlBa Si Al Ba 13-13.5 0.35 145 215 2.5-5
35-40 12-16 9-15
SiCaBaAl Si Ca 13-13.5 0.35 145 225 2.5-5
30-45 9-14
ReSiMg Mg Re Ba Ca Si 13-13.5 0.35 145   2.5-5
5-10 1-5 1-3 2-4 30-50
Ti TI 13-13.5 0.35 145 510 2.5-5